Communications - Scientific Letters of the University of Zilina 2012, 14(4):37-42 | DOI: 10.26552/com.C.2012.4.37-42
Corrosion-Erosion Waste of Metals in the Duct System of the Recycling Aluminium Furnace
- 1 Department of Materials Engineering, Faculty of Mechanical Engineering, University of Zilina, Slovakia
- 2 Department of Power Engineering, Faculty of Mechanical Engineering, University of Zilina, Slovakia
The corrosion aggressiveness of the environment in the recycling aluminium furnace duct system is very high. Temperature is in the range from 300 to 900 °C and chemical composition of combustion varies according to treated aluminium waste and flue gas flow is turbulent. These conditions are very complicated for construction metal selection. The aim of the work is to investigate corrosion-erosion behaviour of various construction metals in the operating conditions of the duct system. The metals with different chemical composition (unalloyed construction steel, stainless steel and nickel based alloy) were tested by long time experiment in the real work conditions of the recycling aluminium furnace. The character and intensity of the materials corrosion attack after one year exposition are evaluated by gravimetric and metallographic analysis.
Keywords: high temperature corrosion, fuel gas, recycling furnace, erosion
Published: December 30, 2012 Show citation
| ACS | AIP | APA | ASA | Harvard | Chicago | Chicago Notes | IEEE | ISO690 | MLA | NLM | Turabian | Vancouver |
References
- MOLNAR, L., VIRCIKOVA, E.: Charakteristika emisii znecistujucich latok z technologie pretavovania hlinikových odpadov [Characteristics of Pollutant Emission from the Remelting Aluminium Waste Technology], Acta Montanistica Slovaca, vol. 10, No. 1, 2005, pp. 220-23.
- HOWES, T. E., ROGERS, P. M., LITTLE, J. A., HUTCHINGS, I. M.: Erosion-corrosion of Mild Steel in a Temperature Gradient, Wear1 86187, 1995, pp. 316-324
Go to original source... - ENTWISLE, M. J., GIBB, J., HUTCHINGS, I. M., LITTLE, J. A., MEADOWCROFT, D. B., NINHAM A.J., OAKEY J. AND SIMMS N.: In E. Bachelet et al. (eds.), The Laboratory Simulation of Fluidized Bed Tube Wastage, High Temperature Materials for Power Engineering, Kluwer, Dordrecht, 1990, pp. 239-248.
- PHONGPHIPHAT, A, RYU, CH, YANG, Y. B. A, FINNEY, K. N., LEYLAND, A., SHARIFI, V. N., SWITHENBANK, J., DAVIS, J. R: ASM Speciality Handbook, Heat Resistant Materials, USA, ISBN 0871705966, 1997.
- BIRKS, N. et al: High Temperature Oxidation of Metals, 2nd edition, Cambridge University Press, 2006, ISBN-13 978-0-521-48042-0
- KHANA, A., S.: High Temperature Oxidation and Corrosion, ASM International, USA 2002, ISBN 0-87170-762-4.
- HADZIMA B., LIPTAKOVA, T.: Zaklady elektrochemickej korozie kovov [Fundamentals of Electrochemical Metal Corrosion], EDIS ZU Zilina, 2008. ISBN 978-80-8070-876-4.
- CERNY M. et al: Korozni vlastnosti kovovych konstrukcnich materialu [Corrosion Properties of Metal Construction Materials], SNTL Praha, 1984.
- NORLING, R., OLEFJORD, I.: Erosion-Corrosion of Fe- and Ni-based Alloys at 550 °C, Wear 254, 2003, pp. 173-184.
Go to original source... - LIPTAKOVA, T., MALCHO, M., JANDACKA, J.: Corrosion Behaviour of Chosen Construction Metals in the Duct System of the Recycling Aluminium Furnace, Material Engineering, vol. 17, No. 3, 2010, pp. 28-34.
- PHONGPHIPHAT, A., CHANGKOOK, RYU YAO, BIN, YANG, FINNEY, K. N., LEYLAND, A., SHARIFI, V. N., SWITHENBANK, J.: Investigation into High-temperature Corrosion in a Large-scale Municipal Waste-to-energy Plant, Corrosion Science 52, 2010, pp. 3861-3874.
Go to original source... - HIDAKA Y., ANRAKU, T., OTSUKA, N.: Deformation of Iron Oxide Scales Upon Tensile Tests at 700-1280◦, In: Abstract Booklet of 5th Intern. Symposium on High Temperature Corrosion and Protection of Materials, Les Embiez, France, 2000 (pp. 4-A115).
This is an open access article distributed under the terms of the Creative Commons Attribution 4.0 International License (CC BY 4.0), which permits use, distribution, and reproduction in any medium, provided the original publication is properly cited. No use, distribution or reproduction is permitted which does not comply with these terms.