Communications - Scientific Letters of the University of Zilina 2012, 14(4):43-47 | DOI: 10.26552/com.C.2012.4.43-47

Microstructural Analysis of Nickel Superalloy MAR-M247

Petr Jonsta1, Zdenek Jonsta1, Katerina Konecna1, Miriam Gabcova1, Karel Hrbacek2
1 VSB-Technical university of Ostrava, Faculty of Metallurgy and Materials Engineering, Czech Republic
2 Prvni brnenska strojirna Velka Bites, a.s., Czech Republic

This paper presents the results of a microstructural phase analysis of the nickel superalloy MAR M247 after casting and different modes of dissolving annealing in the range of 900°C - 1240°C with cooling in water. The alloy in question presents a polycrystalline nickel creepresistant alloy usable especially for highly stressed components in the aerospace and rocket industries. The analysis was performed using a JEOL JSM 6490LV scanning electron microscope with an Oxford Inca x-act x-ray microanalyzer. The presence of minority phases was identified. The study is focused on their possible changes after the application of different modes of thermal treatment.

Keywords: superalloy, phase analysis, annealing

Published: December 30, 2012  Show citation

ACS AIP APA ASA Harvard Chicago Chicago Notes IEEE ISO690 MLA NLM Turabian Vancouver
Jonsta, P., Jonsta, Z., Konecna, K., Gabcova, M., & Hrbacek, K. (2012). Microstructural Analysis of Nickel Superalloy MAR-M247. Communications - Scientific Letters of the University of Zilina, 14(4), 43-47. doi: 10.26552/com.C.2012.4.43-47
Download citation

References

  1. HERNAS, A., JONSTA, Z., et.al: Zarupevne oceli a slitiny [Refractory Steels and Alloys]. 2nd ed. ES VSB-TU Ostrava, 2009, 392 p. ISBN 978-80-248-2187-0.
  2. HRBACEK, K.: Vyzkum a vyvoj technologie presneho liti lopatek stacionarnich plynovych turbin, umoznujici nahradu kovanych lopatek za lopatky lite [Research and Development of Technology of Precision Casting of Blades for Stationary Gas Turbines, Enabling Replacement of Forged Blades by Cast Blades]. Research Report, PBS Velka Bites, 2005, 40 p.
  3. HRBACEK, K.: Soucasny stav vyzkumu a vyvoje superslitin na bazi niklu pouzivanych v nasi republice na casti plynovych turbin, turbodmychadel a odlitky pro sklarsky prumysl [Current State of Research and Development of Nickel-based Superalloys used in the Czech Republic for Components of Gas Turbines, Turbo-blowers and Castings for Glass Industry]. Research Report, PBS Velka Bites, 2004-10-15, 26 p.
  4. LIAO, J., H., et al: Effects of Rhenium on Microstructure and Phase Stability of MAR-M247 Ni-Base Fine-Grain Superalloy. Mat. Trans, vol. 51, No. 4 2010, pp. 810-817. Go to original source...
  5. DONACHIE, M., J., DONACHIE, S., J.: Superalloys: A Technical Guide, 2nd ed. USA, 2002, 439 p. ISBN 0-87170-749-7. Go to original source...
  6. BOR, H., Y., HSU, C., WEI, C., N.: Influence of Hot Isostatic Pressing on the Fracture Transitions in the Fine Grain MAR-M247 Superalloys, Materials Chemistry and Physics, vol. 84, No. 2-3, 2004, pp. 284-290. Go to original source...
  7. CHEN, J. et al: MC Carbide Formation in Directionally Solidified MAR - M247 LC Superalloy. Mat. Sci Eng. A247, 1998, pp. 113-125. Go to original source...
  8. ROKOSZ, S., STASZEWSKI, M., CVAJNA, J. A Complex Procedure for Describing Porosity in Precision Cast Elements of Aircraft Engines Made of MAR-M247 and MAR-M509. Mat. Characterization 56, 2006, pp. 405-413. Go to original source...

This is an open access article distributed under the terms of the Creative Commons Attribution 4.0 International License (CC BY 4.0), which permits use, distribution, and reproduction in any medium, provided the original publication is properly cited. No use, distribution or reproduction is permitted which does not comply with these terms.