Communications - Scientific Letters of the University of Zilina 2021, 23(4):B250-B256 | DOI: 10.26552/com.C.2021.4.B250-B256

Nanoindentation as a Method for Determining the Mechanical Properties of Cold Spray Coatings

Medard Makrenek ORCID...1
1 Faculty of Management and Computer Modelling, Kielce, Poland

The paper presents the methodology behind the statistical selection of input parameters using the example of spraying two cold-sprayed coatings. The Ti and Cr3C2-25(Ni20Cr)-Gr coatings were tested. Despite the large difference in the structure of these coatings, nanoindentation studies were carried out focusing on the nano hardness H and elastic modulus E. Based on the four input parameters and two output parameters, a 2-level factorial 2(k-p) experimental design was performed. The conducted analysis showed the significant influence of the spray distance on the H and E values in the case of the Ti coating. The input parameters of the spray distance and the type of carrier gas used turned out to be statistically significant in the case of the cermet coating. Taking into account the statistical analysis, the coatings were sprayed with modified values of the input parameters.

Keywords: nanoindentation; hardness; elastic modulus; cold spray; 2-level factorial statistics

Received: October 22, 2020; Accepted: January 11, 2021; Prepublished online: June 23, 2021; Published: October 1, 2021  Show citation

ACS AIP APA ASA Harvard Chicago Chicago Notes IEEE ISO690 MLA NLM Turabian Vancouver
Makrenek, M. (2021). Nanoindentation as a Method for Determining the Mechanical Properties of Cold Spray Coatings. Communications - Scientific Letters of the University of Zilina, 23(4), B250-256. doi: 10.26552/com.C.2021.4.B250-B256
Download citation

References

  1. PAWLOWSKI, L. The science and engineering of thermal spray coatings. 2. ed. Chichester: J. Willey & Sons Ltd, 2008. ISBN 0471490490. Go to original source...
  2. SCENDO, M., ZORAWSKI, W., STASZEWSKA, K., MAKRENEK, M., GORAL, A. Influence of surface pretreatment on the corrosion resistance of cold sprayed nickel coatings in acid chloride solution. Journal of Materials Engineering and Performance [online]. 2018, 27(4), p. 1725-1737. ISSN 1059-9495. Available from: https://doi.org/10.1007/s11665-018-3298-6 Go to original source...
  3. ZORAWSKI, W., MAKRENEK, M., GORAL, A. Mechanical properties and corrosion resistance of HVOF sprayed coatings using nanostructured carbide powders. Archives of Metallurgy and Materials [online]. 2016, 61(4), p. 1839-1846. ISSN 1733-3490. Available from: https://doi.org/10.1515/amm-2016-0297 Go to original source...
  4. OTMIANOWSKI, T., ANTOSZEWSKI, B., ZORAWSKI, W. Local laser treatment of tribological plasma sprayed coatings. In: 15th International Thermal Spray Conference: proceedings. 1998. p. 1333-1336. Go to original source...
  5. MAKRENEK, M., BELKA, R., ZORAWSKI, W., KOWALSKI, SZ., SZTORC, M., GORAL, A. Physical and mechanical properties of hydroxyapatite plasma sprayed materials applied in implantology. Medycyna Pracy [online], 2018, 69(6), p. 651-661. ISSN 0465-5893, eISSN 2353-1339. Available from: https://doi.org/10.13075/mp.5893.00725 Go to original source...
  6. WOLFE, D. E., EDEN, T. J., POTTER, J. K., JAROH, A. P. Investigation and characterization of Cr3C2-based wear-resistant coatings applied by the cold spray process. Journal of Thermal Spray Technology [online]. 2006, 15(3), p. 400-412. ISSN 1059-9630. Available from: https://doi.org/10.1361/105996306X124400 Go to original source...
  7. MRDAK, M. Mechanical properties and microstructure of vacuum plasma sprayed Cr3C2-25(Ni20Cr) coatings. Vojnotehnicki Glasnik / Military Technical Courier. 2015, 63(2), p. 47-63. ISSN 0042-8469, eISSN 2217-4753. Go to original source...
  8. PHARR, G. M., HARDING, D. S., OLIVER, W. C. Measurement of fracture toughness in thin films and small volumes using nanoindentation methods. In: Mechanical properties and deformation behavior of materials having ultra-fine microstructures. Nastasti, M. Parkin, D. M., Gleiter, H. (eds.). Dordrecht, the Netherlands: Kluwer Academic Publishers, 1993. ISBN 978-94-011-1765-4, p. 449-461. Go to original source...
  9. GORAL, A., ZORAWSKI, W., MAKRENEK, M. The effect of the standoff distance on the microstructure and mechanical properties of cold sprayed. Surface and Coatings Technology [online]. 2019, 361, p. 9-18. ISSN 0257-8972. Available from: https://doi.org/10.1016/j.surfcoat.2019.01.006 Go to original source...
  10. STEPIEN, A., SITARZ, M., LESNIAK, M. A Sustainable autoclaved material made of glass sand. Buildings [online]. 2019, 9(11), 232. eISSN 2075-5309. Available from: https://doi.org/10.3390/buildings9110232 Go to original source...
  11. CHROMIK, R. R., ZHANG, Y. Nanomechanical testing of third bodies. Current Opinion in Solid State and Materials Science [online]. 2018, 22(4), p. 142-155. ISSN 1359-0286. Available from: https://doi.org/10.1016/j.cossms.2018.05.001 Go to original source...
  12. HINTSALA, E. D., HANGEN, U., STAUFFER, D. High-throughput nanoindentation for statistical and spatial property determination. JOM [online]. 2018, 70(4), p. 494-503. ISSN 1047-4838, eISSN 1543-1851. Available from: https://doi.org/10.1007/s11837-018-2752-0 Go to original source...
  13. COOK, R. D. Detection of influential observations in linear regression. Technometrics [online]. 1977, 19(1), p. 15-18. ISSN 0040-1706, eISSN 1537-2723. Available from: https://doi.org/10.1080/00401706.1977.10489493 Go to original source...

This is an open access article distributed under the terms of the Creative Commons Attribution 4.0 International License (CC BY 4.0), which permits use, distribution, and reproduction in any medium, provided the original publication is properly cited. No use, distribution or reproduction is permitted which does not comply with these terms.